Definition of Powder Coating vs. Liquid Coating for Die Castings
Liquid coating uses solvent-borne or water-borne paint applied by spray gun, often as a primer followed by a topcoat. Each dry coat is typically 20 to 40 µm, and the paint cures at room temperature or in a low-temperature oven. Both finishes are specified by resin type, color reference, gloss level and film thickness, which is measured on aluminum with an eddy-current gauge.
Why This Matters for Your Business
Liquid paint is often the better option for small batches in several colors, for matching the color of an existing product, and for parts where a heavy film would interfere with assembly. Powder lines are less flexible here, because each color change means cleaning the booth, and many coaters set a minimum quantity per color. The higher curing temperature of powder also makes porosity in the casting more likely to show as surface defects.
Whichever finish you choose, the RFQ should state the color standard and gloss, the film thickness range, the surfaces to be masked, such as threads and machined bores, and the adhesion and corrosion tests the parts must pass. A finish described only as "black paint" on the drawing tends to vary between batches and between suppliers.
Related Terms
conversion coating electro coating casting porosity surface roughness shot blasting maskingFAQ
Why do powder coated aluminum die castings sometimes show pinholes or blisters after curing?
Gas trapped in porosity just below the casting skin expands in the curing oven and escapes through the soft powder film, leaving pinholes, craters or small blisters. Liquid paint cures at a lower temperature, so the same casting may look acceptable when painted. The usual remedies are to pre-bake the castings above the powder's cure temperature before coating, so that the gas escapes first, and to use a degassing grade of powder. Where the porosity sits under a cosmetic surface, the lasting fix is in the casting process, through changes to gating and venting or the use of vacuum assistance. You should ask the supplier how porosity in coated faces is found within its quality inspection process.
How well do powder and liquid paint cover sharp edges and deep recesses on die cast parts?
Both thin out on sharp edges, and powder has the most difficulty in deep recesses and inside corners, where the electrostatic field keeps the powder from reaching the surface (the Faraday cage effect). Liquid paint reaches recesses more easily but draws away from edges as it dries. The simplest remedy is an edge radius of at least 0.5 mm, which is easiest to add at the mold design stage. Edge-cover powder grades help where the geometry cannot change.
How can I verify paint adhesion on die cast parts before approving a coating supplier?
Ask for cross-cut adhesion results to ISO 2409 on production parts, not only on test panels, with class 0 or 1 as the usual acceptance level. The test cuts a lattice through the film and checks how much coating lifts off with tape. Adhesion on aluminum depends mainly on pretreatment, so ask which conversion coating the coater uses and how its bath is monitored. Agree the neutral salt spray hours to ISO 9227 at the same time. A supplier with ISO 9001:2015 quality credentials should keep these records for each batch.