If your heat sink is ready to go out for quotation, several parts of a die cast aluminum heat sink design are far easier to decide before the tool is built than afterward. They are the alloy, the fin geometry, the way the face under your LED board or power device is machined and finished, and what your drawing tells the foundry about each. A major change to a tool’s geometry once production has started can mean welding and re-machining the steel, which can affect your production schedule. This article takes each decision in turn.
We cast heat sinks and controller housings to our customers’ own designs at our facility in Changhua, Taiwan, for brands in the USA and Europe making LED systems, power electronics and telecommunications equipment. Our page on aluminum heat sink and controller housing die casting shows the kinds of parts involved. The thermal design is your team’s work; what follows is the casting side of it, and the points where we’ll ask you to decide something.
Which aluminum alloy gives your die cast heat sink the best thermal conductivity?
The North American Die Casting Association (NADCA) lists alloy 360 at 113 W/m·K and alloys 380 and 383 at 96.2 W/m·K in its Product Specification Standards for Die Castings. Those are the two alloys we cast, and the difference between them is about 17%. You may find other conductivity figures quoted for the same alloys, some of them noticeably lower or higher, so it helps to ask any supplier which source a figure comes from before you use it in a thermal calculation. The figures in this article come from NADCA.
ADC-12 / A383 for most heat sinks
ADC-12 / A383 is our standard recommendation for most heat sink work, because it offers a good balance of thermal conductivity, castability and cost. NADCA rates it 1 for die filling, the best score on its scale. On a heat sink that rating shows in the fins, where the metal has to reach the tip of every fin before it solidifies. Our glossary entry on ADC-12 castability covers the alloy in more detail.
A frequent misconception, when a drawing was first written for a North American foundry, is that A380 and ADC-12 are the same alloy. A380 corresponds to ADC10 under the Japanese standard, and ADC-12 corresponds to A383, as our reference on die casting alloy names across regions explains. If your drawing calls for A380, please tell us whether ADC-12 / A383 is acceptable to you, since those two alloys share the same NADCA conductivity figure and ADC-12 is the one we pour.
When ADC-3 / A360 is the better choice
A360 conducts better and resists corrosion better (NADCA rates it 2 for corrosion resistance against 3 for A383), but it’s rated 3 for die filling and is harder to cast. Its strength comes from magnesium rather than copper, and NADCA describes the principal disadvantage of copper in these alloys, in its aluminum alloy data, as its marked effect on corrosion resistance. We use ADC-3 / A360 for our marine work. For a heat sink that will be installed near the sea, or one where the extra conductivity makes a real difference to your thermal margin, we would suggest raising A360 at quotation. Our engineers can then tell you whether your fin layout will fill reliably in that alloy before you commit to it. The ADC-3 corrosion resistance entry in our glossary explains where the alloy’s advantage comes from.
| ADC-12 / A383 | ADC-3 / A360 | |
|---|---|---|
| Thermal conductivity (NADCA) | 96.2 W/m·K | 113 W/m·K |
| Die filling (NADCA, 1 is best) | 1 | 3 |
| Corrosion resistance (NADCA, 1 is best) | 3 | 2 |
| How we use it | Standard alloy for heat sink and controller housing work | Marine work; to discuss where conductivity or a corrosive site matters more |
Our guide to choosing an aluminum alloy for die casting compares these with three other common alloys.
What fin geometry your die cast heat sink needs to fill reliably
Our die casting team works to an average wall thickness of 2.5 to 4.5 mm, depending on part size and flow length, and walls below 1.5 mm risk incomplete fill or weak sections. A fin behaves much like a thin wall in this respect, since the metal enters at the root and has to travel to the tip, losing heat to the die the whole way. The design question is usually how far the fins can be thinned for surface area before they stop filling completely.
Fin thickness, height and the base
How thin a fin can be depends on its height, its spacing and where the metal enters the tool, so a single minimum figure would mislead you. We would rather determine it on your own geometry. If you send us the CAD model while the fin array can still change, our mold engineers will tell you which fins are likely to fill and which need more thickness or draft.
The base plate needs the same attention from the other direction. A thick base helps spread heat from a concentrated source, but heavy sections tend to shrink and develop porosity as they cool, which is why our guidance is that walls should generally not exceed 15 mm. If your thermal design calls for a heavy base, we can look at it with you at quotation, along with options such as ribs or pockets on the non-contact side.
Gates, fill and porosity at the fin roots
Our mold engineers run mold flow simulation before the mold is made. The simulation predicts how the metal fills the fins, where porosity is likely to form and how the gates and runners should be sized, and we share the report with you at the mold design review. Gate placement and venting can then be arranged to direct porosity away from critical areas.
On a heat sink, one critical area is the contact face, because porosity close to the surface can be opened up when the face is machined. Mark the contact face clearly on your drawing, and our engineers will treat it as a critical area in the simulation as well as on the machine. Our glossary entry on shot parameters and metal fill rate explains the injection side of the process.
How the contact face of your heat sink is machined and finished
Critical mounting surfaces on our heat sinks are CNC machined after casting to the flatness your thermal interface requires, and we verify flatness and mounting hole positions on a CMM before the parts ship. Our article on machining an LED mounting face for flatness covers the flatness question in more detail, including how a large flat face can move after machining.
Machining the contact face
We machine heat sinks on our CNC machining centers, all of which have fourth-axis capability, in a temperature-controlled facility. Two things on your drawing help us most here. The first is the datum the contact face relates to, since flatness on its own doesn’t tell us how the face sits relative to the mounting holes. The second is the surface roughness you need on the face, stated as an Ra value, which we can check on our roughness tester. Our entry on surface roughness specification explains how Ra is defined and measured.
Choosing a finish for a heat sink
We offer five surface treatments in house: powder coating, electro-coating, liquid coating, anodizing and SurTec 650 trivalent chromium. For heat sinks, trivalent chromium is the most common choice, as it improves corrosion resistance without significantly affecting thermal conductivity. Powder coating suits a heat sink or housing that needs a specific color or more environmental protection.
It’s possible to anodize ADC-12, but NADCA rates both A380 and A383 at 3 for anodizing appearance. That’s acceptable for a functional finish, though it won’t give you a bright, even decorative surface.
Whichever finish you choose, the drawing should say whether the contact face is to be left bare. We can then agree with you how that face is protected during finishing, before the tool is made.
What to include when you send a heat sink design for quotation
Our mold engineering team reviews your CAD files during quotation and returns DFM recommendations on draft angles, wall thickness uniformity, gate placement and geometry. We also calculate the machine tonnage your heat sink needs from its projected area at that stage, as our entry on machine tonnage selection explains.
What your drawing should state
Along with the CAD model, these are the points that help our engineers most:
- The contact face, marked as functional, with its flatness, its roughness and the datum it relates to
- Faces that are cosmetic only, and any where gate or ejector marks would be a problem
- The finish, and any bare areas
- The alloy, or a note that you would like our recommendation
- Your expected annual volume, since it affects the tool we propose
On size, we cast parts from 5 grams to 3 kilograms on 12 machines from 135 to 900 tons, and the 900 ton machine takes castings up to 700 mm. Our hanger shot blaster takes parts up to 600 mm, so for a coated heat sink longer than that, please confirm the finishing route with us at quotation.
What we check before your heat sinks ship
Before production starts, our quality team carries out first article inspection on two Mitutoyo CMMs and a Keyence 3D scanner, and sends you the report and physical samples for approval. We check incoming ingot on our spectrometer, and every shipment comes with material certification and CMM data for the critical features. Coated parts can also be salt spray tested.
Thermal performance is measured on your assembled product, by your team. What our records give you is confirmation of the alloy, the dimensions and the finish that your thermal validation depends on.
If you send us the CAD model and drawing for your heat sink, with your annual volume and the finish you have in mind, our mold engineers will review it and come back with their comments on alloy, fin fill and the contact face before we quote.
Frequently asked questions about die cast aluminum heat sink design
Which alloy do you use for die cast heat sinks?
ADC-12 / A383 is the standard alloy for die cast aluminum heat sinks, because it fills fine fin geometry reliably and offers a good balance of thermal conductivity and cost. ADC-3 / A360 is the alternative where higher conductivity or better corrosion resistance is needed and the fin layout can still be filled in that alloy.
What is the thermal conductivity of ADC-12?
NADCA lists alloy 383, the North American equivalent of ADC-12, at 96.2 W/m·K, the same figure it gives for alloy 380. Alloy 360, the equivalent of ADC-3, is listed at 113 W/m·K. Conductivity figures for these alloys vary between sources, so you should check where any figure used in a thermal calculation comes from.
How thin can heat sink fins be in aluminum die casting?
The minimum fin thickness for an aluminum die cast heat sink depends on fin height, spacing and gate position, so it’s best determined on the actual geometry. Average walls of 2.5 to 4.5 mm are typical, and walls below 1.5 mm risk incomplete fill. Mold flow simulation before the tool is made shows which fins will fill.
Can the contact face of a heat sink be left uncoated?
The contact face of a coated heat sink can be kept bare, provided the drawing states it. The protection method for that face during finishing should then be agreed with the foundry before the tool is made.
Can you cast a heat sink in A360 instead of ADC-12?
A heat sink can be cast in ADC-3 / A360, which NADCA lists at 113 W/m·K against 96.2 W/m·K for ADC-12 / A383. A360 is harder to fill, so dense or tall fins should be checked with mold flow simulation before the alloy is confirmed.