Definition of Electro Coating for Aluminum Die Castings
This gives an even thickness of typically 15 to 30 µm, including inside recesses and holes. The parts are then rinsed and baked, usually at 160 to 180 °C. E-coat is specified by resin type (epoxy or acrylic), color, film thickness and the salt spray hours the coated part must withstand.
Why This Matters for Your Business
The thin, even film also saves cost at assembly. Threads, press-fit bores and mating faces often need no masking and no rework, which reduces handling and the risk of fit problems that heavier finishes can cause.
Please state in the RFQ (request for quotation) whether e-coat is the final finish or a primer, together with the resin type, color, thickness range and corrosion test requirement. The parts hang on racks that carry the current, so the drawing should also show where a small uncoated contact mark is acceptable.
Related Terms
conversion coating salt spray testing casting porosity powder coating shot blasting maskingFAQ
When does e-coating offer a practical advantage over powder or spray painting on aluminum castings?
E-coating has the advantage when the part has recesses, ribs, blind holes or internal passages that a spray gun cannot reach, since the current carries paint to every surface the bath touches. On flat, open shapes in a decorative color, other finishing options for aluminum parts are usually simpler and cheaper.
Can e-coated aluminum parts be used outdoors without a topcoat?
Epoxy e-coat should not be the only finish on parts exposed to sunlight, because ultraviolet light breaks down the resin and the surface chalks and fades over time. Its corrosion protection is good, but its resistance to sunlight is poor. Acrylic e-coat is made for exterior use as a single coat and holds its color and gloss better, although its corrosion resistance is usually somewhat lower than that of epoxy. For agricultural machinery components and other parts left in the open, the usual choices are acrylic e-coat alone or epoxy e-coat under a powder topcoat. Please confirm which resin your coater runs, since one tank normally holds only one.
What causes bare spots, craters or poor adhesion when electro coating die cast aluminum?
Most of these faults start with the surface before coating. Die release agent left from casting, and cutting fluid from machining, block the conversion coating and leave bare or poorly bonded areas, so degreasing has to remove both. High-silicon alloys such as ADC12 leave a dark silicon smut after etching, which must be removed with a desmut step, a short acid dip, or adhesion suffers. Craters and pinholes after baking usually come from gas escaping out of surface porosity, which a pre-bake or better casting control reduces. Release agent is chosen and applied during die casting production, so it is worth asking the caster and the coater to agree on one that cleans off reliably. You should also ask for cross-cut adhesion results on parts from each new lot.